What this inspection covers
A panel may need to sit flat against a mating surface, while a sealing or finished surface may also have a roughness requirement. These are different checks. Identify the surface and requirement on the drawing, then choose the flatness or Ra method described below.
If the source of dimensional limits is unclear, follow the checking steps in the general tolerance guide and ask the person responsible for the drawing or contract to confirm the requirement. The guide does not replace that approval or establish a default class; method suitability still needs confirmation for the feature and agreed requirement.
For flatness, keep support and restraint conditions consistent. For Ra, confirm measurement direction and instrument settings. Record these conditions with the readings so results from different pieces or process stages can be compared.
Flatness: what it measures
Flatness is how far a surface departs from a plane. On sheet metal it shows up as a bow, a twist or a panel that rocks on a surface plate. A flatness requirement belongs on the drawing when the part has to sit against another surface, seal, or assemble without being forced.
Checking flatness
- A surface-plate check must also meet the applicable requirement. A straightedge and feeler gauge are for screening only and do not automatically constitute a full specified flatness evaluation; use the method confirmed for that requirement.
- Measure after the last cutting or welding operation, not only after the first cut.
- Record the nesting and the cut sequence with the result, because a flat part from one layout does not prove the next layout.
- Where stress relief is used, record the operation and check flatness again afterwards.
- State flatness on the drawing when it matters. An unstated requirement leaves the workshop without a limit, and an unnecessary tight value adds handling and rework.
Three causes of lost flatness
Flatness is affected by residual stress, by nesting and by cutting heat input.
- Residual stress can be present in the incoming sheet and is released when material is removed, so a nested layout that removes more material from one side can pull the part out of plane.
- Nesting changes how much material is removed and where, so it changes the balance of stress in the part.
- Cutting heat input adds a local stress pattern, especially on long contours and close nests. Welding adds a larger one.
- Stress relief and a considered sequence reduce the effect, but they do not make an unstable layout stable.
For the cutting process behind heat input and nesting, see laser cutting.
Surface finish: Ra and the drawing
Surface finish describes how rough or smooth a surface is at a small scale. Ra is the common roughness parameter: it summarises the height of the small peaks and valleys over the measured length. A drawing or customer requirement should state the Ra value and the surface it applies to. A generic workshop table can help a discussion, but it cannot replace that requirement.
Measuring surface finish
- Read the drawing note for the Ra value, the parameter and the surface it applies to before measuring.
- Identify the surface that carries the requirement: a cut edge and a formed face are different surfaces.
- Use the instrument and setup required for the applicable method. Confirm the measurement direction, filtering and evaluation length from that method or the agreed requirement; if unspecified, ask for confirmation before measuring.
- Measure at the location that matters, not at the most convenient part of the surface.
- Record the method with the result so a later comparison uses the same method.
Before calling a measurement a pass
| Field | Flatness record | Surface roughness record |
|---|---|---|
| Requirement | Drawing revision, surface, limit and agreed method | Drawing revision, parameter, value/unit and measured surface |
| Setup | Part free or restrained; support points; orientation; process stage | Instrument/stylus, direction, filtering and evaluation length required by the method |
| Readings | Marked locations and original readings; repeat under the same support | Trace/location IDs and original readings, not a visual finish description |
| Decision | Compare by the agreed method; flag uncertain or conflicting results | Do not substitute an average from a different surface or setup |
Use a straightedge and feeler gauge for an initial workshop check when suitable. A specified full flatness evaluation may require a different method. Supporting or clamping a thin panel changes its shape, so retain the support and restraint conditions with each result.
The inspection record
A result without a method cannot be compared. Record the requirement, the surface, the measurement location, the instrument and the sequence or nesting state for each check. Keep the record with the part or the batch so a later change can be separated from a process fault.
Suggested records should link the order, part or batch ID, drawing revision and requirement source to the actual method, conditions and original readings. Mark missing information as awaiting confirmation. Methods stated in the drawing, contract or customer confirmation must relate to the same inspection requirement; ask the responsible person to clarify conflicts rather than assuming a universal order of precedence.
Before purchase, agree the inspection items, methods, sampling quantity/frequency and records to be delivered; see quality and inspection agreements. This agreement must stay linked to the same requirement and does not create a separate default technical method. Suggested fields and a blank template cannot replace an original report with actual conditions and readings for the identified part or batch.
Where to go next
General tolerances explain how the drawing states limits. The defect atlas links symptoms to possible causes and checks that narrow the investigation. ISO 9013 guide covers thermal cut-edge classification, a separate description of edge quality.